Research Article

Simultaneous and Gradient IPN of Polyurethane/Vinyl Ester Resin: Morphology and Mechanical Properties

Figure 2

Strain-stress curves of g-IPN with different component sequences at different time intervals: (a) hours and (b) hours.
514124.fig.002a
(a)
514124.fig.002b
(b)