Research Article

Improved Field Emission Characteristics of Large-Area Films of Molybdenum Trioxide Microbelt

Figure 4

Optical images of the site distribution of the MoO3 microbelt films grown with different separation of substrate and evaporation source: (a) 27 cm, (b) 32 cm, and (c) 37 cm under similar gap fields: (a) 𝐸 = 5 . 4 3  V/ 𝜇 m, (b) 𝐸 = 5 . 4 3  V/ 𝜇 m, (c) 𝐸 = 5 . 4 7  V/ 𝜇 m, the corresponding substrate areas are 0 . 4 5 c m × 0 . 5 c m , and 0 . 4 5 c m × 0 . 5 c m and 0 . 4 5 c m × 0 . 5 c m , respectively. (The sample area is indicated by the dashed line.)
136860.fig.004a
(a)
136860.fig.004b
(b)
136860.fig.004c
(c)