Research Article

Nanocomposite Materials of Alternately Stacked Monolayer and Graphene

Figure 1

XRD intensity from as-prepared samples. (a) XRD intensity from graphite oxide (GO) and alkylamine-intercalated graphite oxides (GO-amine) with different chain lengths ( C 𝑛 H 2 𝑛 + 1 N H 2 ) ( 𝑛 = 3 - 8 ) . The peaks of GO and GO-amine are indicated by the arrows in the figure. (b) XRD intensity from GO-amine with different chain lengths in C 6 0 solution ( 𝑛 = 3 - 8 ) .
891514.fig.001a
(a)
891514.fig.001b
(b)