Research Article

Direct Deposition of Micron-Thick Aligned Ceramic Nanofibrous Film on FTOs by Double-Needle Electrospinning Using Air-Turbulence Shielded Disc Collector

Figure 1

(a) Experimental setup of electrospinning. The metal oxide precursor is taken in a syringe. 1-mm-thick six FTOs are fixed on the holder mounted on rotating disc at equal space. The rotating disc of diameter 20 cm with (b) top-shield, (c) enclosed-air-shield, (d) enclosed-air-shield with air-hood (front view), and (e) air-hood arrangement (top view) for the turbulent air to escape.
739241.fig.001a
(a)
739241.fig.001b
(b)
739241.fig.001c
(c)
739241.fig.001d
(d)
739241.fig.001e
(e)