Research Article

The Low-Temperature Crystallization and Interface Characteristics of ZnInSnO/In Films Using a Bias-Crystallization Mechanism

Figure 4

The resistivity and crystallization of unbiased ZITO/In sample and ZITO/In sample with biased of 4 V for 20 min.