Microstructure and Crystallization Kinetics of Polyurethane Thermoplastics Containing Trisilanol Isobutyl POSS
Figure 4
Crystallization thermograms obtained at a cooling rate of 10°C·min−1 after removal of the thermal history carried out at a heating rate of 10°C·min−1 from −50 to 240°C.