Basic Potential of Carbon Nanotubes in Tissue Engineering Applications
Figure 6
Viability of BEAS-2B cells treated with different MWCNTs. The cells were exposed to MWCNTs for 24 h. The graph shows the cell viability associated with 10 μg/mL of each MWCNT in the MWCNT-150 and MWCNT-80 series (mean ± SE, , , ). The table shows the basic properties of the MWCNTs [54].