Research Article

Lithium Ion Storage Characteristics of Mechanically Fractured Titanate Nanotubes

Figure 4

Initial charge/discharge profile of titanate nanotubes with the milling condition of 0, 15, 30, 45 and 60 minutes at a current rate of 10 mA·g−1 between 1.0 and 3.0 V.
394089.fig.004