Research Article

Effect of Titanium Substitution on Magnetic Properties and Microstructure of Nanocrystalline Monophase Nd-Fe-B Magnets

Table 1

Magnetic properties of Nd12.3Fe81.7βˆ’xTixB6 ( π‘₯ = 0 . 5 , 1 . 0 , 2 . 0 , 3 . 0 ) ribbons annealed at 600Β°C for 10 min.

π‘₯ ( 𝐡 𝐻 ) m a x (kJ/m3) 𝐻 c i (kA/m) 𝐽 π‘Ÿ (T) 𝐽 π‘Ÿ / 𝐽 𝑠

0.576.2616.10.790.73
1.0151.6809.21.020.74
2.096.7730.20.860.71
3.084.5777.20.850.67