Research Article

The Investigation of Bioactivity and Mechanical Properties of Glass Ionomer Cements Prepared from Al2O3-SiO2 Glass and Poly(γ-glutamic acid)

Figure 3

TF-XRD patterns of the surface of SBF-unsoaked cement prepared by the -PGA concentration of 10% m/m and P/L ratio of 1 : 1, the Al2O3-SiO2 glass powders, and the surfaces of cements prepared by different concentration of -PGA solution using P/L ratio of 1 : 1, after soaking in SBF for 7 days.
168409.fig.003