Research Article

TiO2 Deposition on AZ31 Magnesium Alloy Using Plasma Electrolytic Oxidation

Table 2

Electrochemical parameters of AZ31 substrate and PEO coating after 5-minute treatment.

Sample (V) (A/cm2) (V) (V) cm2) C.R. (mpy)

AZ31−1.465 0.1650.10311.25
PEO−1.418 0.0410.074