Research Article

Experimental Investigation on the Durability of Glass Fiber-Reinforced Polymer Composites Containing Nanocomposite

Figure 13

The SEM images of fracture surface of VE-GFRP immersed in alkaline solution for 45 days.
352639.fig.0013