Processing of CNTs Reinforced Al-Based Nanocomposites Using Different Consolidation Techniques
Figure 9
SEM micrographs of as-received Al-12Si-0.3Mg (alloy 2) and sintered at 500°C using (a) microwave, (b) hot isostatic pressing (HIP), and (c) Spark plasma (SPS) sintered samples.