TG data of PS and PS/organo-MMT nanocomposites at different sonication times.

Samples (°C)Weight loss %DTG Char %

PS388.071004300
PS/10MB2/0.5 h443.5485.11945714.881
PS/10MB2/1 h444.7584.89246015.108
PS/10MB2/1.5 h441.3083.45845316.542