Research Article

Dense Nanostructured Nickel Produced by SPS from Mechanically Activated Powders: Enhancement of Mechanical Properties

Figure 6

Dilatometric curves of sintering of the commercial powder (270–1000°C) and the mechanically activated Ni powder (230–800°C).
674843.fig.006