Fabrication of Vertically Aligned CNT Composite for Membrane Applications Using Chemical Vapor Deposition through In Situ Polymerization
Figure 4
(a) Surface morphology of a sample after deposition of polymer by thermal CVD (after 15 minutes). (b) Cross-sectional view of deposited fluorocarbon polymer between vertically aligned MWCNTs (after 40 minutes).