Research Article
A Mucoadhesive Electrospun Nanofibrous Matrix for Rapid Oramucosal Drug Delivery
Table 6
Experimental values obtained from nanotensile analysis.
| Sample | Young’s modulus (MPa) | Yield stress (MPa) | Ultimate strength (MPa) | Ultimate strain | Toughness (J/cm3) |
| Fiber layer | 26.09 | 0.49 | 2.98 | 0.227 | 0.38 | NFMS film | 36.01 | 1.675 | 3.33 | 0.242 | 0.62 | NFMS | 30.31 | 1.18 | 2.79 | 0.238 | 0.48 | FD | 56.35 | 1.13 | 2.73 | 0.314 | 0.71 | FE | 20.34 | 1.10 | 3.52 | 0.731 | 2.10 |
|
|