Dielectric Properties and Characterisation of Titanium Dioxide Obtained by Different Chemistry Methods

Figure 9

The temperature dependence of (a) dielectric constant and (b) loss tangent measured at 1.15 MHz for investigated rutile samples annealed for 2 h at 850°C (synthesis ) and at 900°C (syntheses and (3)).
124814.fig.009a
(a)
124814.fig.009b
(b)