Research Article

Characterization of the Nanoporous Template Using Anodic Alumina Method

Figure 1

Setup for anodic oxidation: (a) experimental apparatus, (b) power supply, and (c) holder.
130716.fig.001a
(a)
130716.fig.001b
(b)
130716.fig.001c
(c)