Research Article

Optical Amplification at 1525 nm in BaYF5: 20% Yb3+, 2% Er3+ Nanocrystals Doped SU-8 Polymer Waveguide

Figure 2

(a) A TEM image of nanocrystals, the average crystals size is about 13 nm. (b) The corresponding histogram of size distribution.
153028.fig.002a
(a)
153028.fig.002b
(b)