Main electrochemical parameters for bare and anodic oxidized Ti-15Ta-5Zr alloy in Ringer solutions at 37°C.
| Parameter | Ringer pH = 3.54 | Ringer pH = 7.49 | Ringer pH = 8.98 | Bare | Oxidized | Bare | Oxidized | Bare | Oxidized |
| (mV) | −350 | −300 | −200 | −150 | −350 | −300 | (mV) | −150 | −150 | −100 | −75 | −200 | −175 | (mV) | >2000 | >2000 | >2000 | >2000 | >2000 | >2000 | (mV) | 200 | 150 | 100 | 75 | 150 | 125 | (A/cm2) | 5.0 | 2.5 | 2.0 | 0.9 | 4.5 | 2.5 |
|
|