EDX results of GNR-grafted TiO2 nanotubes treated by various concentrations of aqueous thiolactic acid solution.
| |
| Weight % | | kV | C | Ti | Au | O |
| (1) 1 M thiolactic acid | 5 | 1.97 ± 0.12 | 51.77 ± 1.95 | 5.74 ± 0.68 | 40.52 ± 1.92 | 10 | 1.73 ± 0.16 | 53.96 ± 0.55 | 3.27 ± 0.44 | 41.05 ± 0.53 | 15 | 1.4 ± 0.14 | 58.03 ± 0.32 | 1.26 ± 0.23 | 41.31 ± 0.30 | 20 | 0.99 ± 0.29 | 57.03 ± 0.50 | 1.12 ± 0.32 | 40.86 ± 0.47 |
| (2) 0.5 M thiolactic acid | 5 | 1.27 ± 0.09 | 52.72 ± 1.84 | 6.61 ± 0.68 | 39.40 ± 1.81 | 10 | 1.61 ± 0.16 | 54.04 ± 0.56 | 3.52 ± 0.45 | 40.83 ± 0.54 | 15 | 1.51 ± 0.18 | 55.65 ± 0.39 | 1.47 ± 0.29 | 41.37 ± 0.37 | 20 | 1.43 ± 0.2 | 53.30 ± 0.33 | 0.76 ± 0.21 | 41.51 ± 0.32 |
| (3) 0.1 M thiolactic acid | 5 | 1.84 ± 0.10 | 47.69 ± 1.68 | 12.23 ± 0.73 | 38.24 ± 1.62 | 10 | 1.79 ± 0.16 | 52.10 ± 0.53 | 5.83 ± 0.46 | 40.28 ± 0.51 | 15 | 1.14 ± 0.20 | 55.82 ± 0.43 | 2.40 ± 0.34 | 40.63 ± 0.41 | 20 | 0.98 ± 0.22 | 56.52 ± 0.37 | 1.91 ± 0.24 | 40.59 ± 0.35 |
|
|