Research Article

Texture-Etched SnO2 Glasses Applied to Silicon Thin-Film Solar Cells

Figure 6

AFM images of SnO2 etched in the etchant A at 90°C for (a) 0, (b) 30, (c) 120, and (d) 300 sec.
907610.fig.006a
(a)
907610.fig.006b
(b)
907610.fig.006c
(c)
907610.fig.006d
(d)