Preparation of Nanostructured Microporous Metal Foams through Flow Induced Electroless Deposition

Figure 11

XRD pattern of the Ni-P structure (same sample in Figure 10) after heat treatment at 600°C. Sample details: plating bath composition: [Ni] = 0.13 M, [P] = 1.26 M and heat treatment conditions: °C, heating rate = 10°C, and curing/annealing time  min followed by cooling in air.