Research Article
Preparation of Nanostructured Microporous Metal Foams through Flow Induced Electroless Deposition
Figure 18
Variation of the cumulative and incremental pore radius with pore size of the crust and bulk. Processing conditions: [Ni] = 0.63 M; [P] = 1.26 M; °C, °C/min; min followed by cooling in air. (a) Crust. (b) Bulk of the monolith.
(a) |