Research Article
Preparation of Nanostructured Microporous Metal Foams through Flow Induced Electroless Deposition
Table 3
Pore size distribution by surface area analysis. Processing conditions: [Ni] = 0.63 M; [P] = 1.26 M, = 600°C, = 10°C/min = 60 min followed by cooling in air.
|