Research Article

Experimental Investigation of the Properties of Electrospun Nanofibers for Potential Medical Application

Table 2

Sample descriptions of EVOH nanofibers.

Sample groupFabrication parametersFibre diameter range

A7.5% solution, 15 kV, 2.5 mL/hr, 0.4–0.9 μm
20 cm standing distance

B10% solution, 15 kV, 2.5 mL/hr, 0.8–1.5 μm
20 cm standing distance

C12% solution, 15 kV, 2.5 mL/hr, 1.3–2.2 μm
20 cm standing distance