Research Article
The Photocatalytic Activity of TiO2-Zeolite Composite for Degradation of Dye Using Synthetic UV and Jeddah Sunlight
Table 1
Crystal lattice analysis of different investigated samples.
| Sample | Phase name | Degree of crystallization | Crystal system | (Å) | (A) | (A) | Alpha (deg) | Beta (deg) | Gamma (deg) |
(Å3) |
| 20% TiO2/FAU | Anatase | 40% | Tetragonal (body centered) | 3.775(17) | 3.775(17) | 9.55(7) | 90.000000 | 90.000000 | 90.000000 | 136.1(13) | 70% TiO2/FAU | Anatase | 100% | Tetragonal (body centered) | 3.7787(15) | 3.7787(15) | 9.504(7) | 90.000000 | 90.000000 | 90.000000 | 135.70(12) | 20% TiO2/LTA | No anatase crystals just LTA | 0 | | 12.2353(4) | 12.2353(4) | 12.2353(4) | 90.000000 | 90.000000 | 90.000000 | 1831.66(10) | LTA | | 0 | | 12.2800(4) | 12.2800(4) | 12.2800(4) | 90.000000 | 90.000000 | 90.000000 | 1851.809 | 70% TiO2/LTA | Anatase | 100 | Tetragonal (body centered) | 3.779(5) | 3.779(5) | 9.486(14) | 90.000000 | 90.000000 | 90.000000 | 135.4(3) |
|
|