The Photocatalytic Activity of TiO2-Zeolite Composite for Degradation of Dye Using Synthetic UV and Jeddah Sunlight
Table 3
Oxide % EDX analysis of different catalyst samples.
| Sample | 20% TiO2/X | 70% TiO2/X | 20% TiO2/A | 70% TiO2/A |
| Theoretical EDX % of oxide | Na2O | 8.75 | 3.04 | 20.17 | 1.62 | Al2O3 | 17.81 | 2.07 | 32.86 | 2.11 | SiO2 | 34.50 | 4.04 | 44.52 | 7.36 | TiO2 | 38.95 | 90.85 | 2.45 | 88.92 |
|
|