Research Article
Structural and Optical Properties of CuInS2 Thin Films Prepared by Magnetron Sputtering and Sulfurization Heat Treatment
Figure 11
SEM micrographs of the samples prepared under the optimized condition: the holding time is 2 h; the sulfurization temperature is 470°C; the sputtering pressure is 0.8 Pa; the sputtering power is 80 W.
(a) |
(b) |