Effects of Chitosan Concentration on the Protein Release Behaviour of Electrospun Poly(-caprolactone)/Chitosan Nanofibers

Table 2

Applied voltage and average nanofibers diameter and pore size in electrospinning PCL/chitosan nanofibers with different BSA%.

BSA VoltageAverage fiber Coefficient of Average pore Coefficient of
wt.%(KV)diameter (nm)deviation (%)size (nm)deviation (%)

518122.45.60387.1921.25
1021133.475.60429.4524.88
1520117.396.74418.4322.71
2021109.955.09490.2425.10