Research Article
Indentations on Air Plasma Sprayed Thermal Barrier Coatings Prepared by Different Starting Granules
Figure 8
Typical Hertzian indentation damage and cracks on the surface of YSZ coatings deposited by APS, using WC sphere radius mm; (a), (b) ring crack damage is found in YZ-WH or YZ-AH and (c) radial crack damage is found in YZ-WD.