Research Article
Preparation of Nanosized LaCoO3 through Calcination of a Hydrothermally Synthesized Precursor
Figure 4
TGA-DSC thermograms of the precursor powder. The calcination temperature used for obtaining each sample is shown for reference: (a) 380, (b) 490, (c) 740, (d) 850, (e) 950°C, and (f) 1050°C.