Research Article

Nanocomposite of CeO2 and High-Coercivity Magnetic Carrier with Large Specific Surface Area

Figure 5

(a, b) The ZFC-FC curves measured at 0.01 T for the CoFe_free, CoFe_mod, and v0x samples, respectively. (c) Distribution of blocking temperatures, (), obtained from the ZFC curve refinement (details about the data analysis can be found in the Supplementary Material).
(a)
(b)
(c)