(a, b) Magnetization isotherms of the CoFe_free and CoFe_mod samples measured at 10 K and 400 K together with refined curves (solid lines) at 400 K. (c) Magnetization isotherms of the nanocomposite samples measured at 10 K. (d) Magnetization isotherms of the nanocomposite samples measured at 400 K together with the refined curves (solid lines).
(a) 10 K
(b) 400 K
(c) 10 K
(d) 400 K