Research Article

Morphological and Rheological Characterization of Gold Nanoparticles Synthesized Using Pluronic P103 as Soft Template

Figure 3

Intensity of the UV-Vis absorbance peak measured at 540 nm versus synthesis temperature for HAuCl4 and P103 aqueous solutions with different concentrations of P103: () 10 wt.%; () 15 wt.%; and () 20 wt.%. Insets show UV-visible scans of HAuCl4-P103 aqueous solutions.