Journal of Nanomaterials / 2017 / Article / Tab 4

Research Article

Sodium Hypochlorite as Fluorotic Dentin Pretreatment of Two-Step Self-Etch Adhesive with Silver Nanoparticle: Atomic Force Microscope and Adhesive Microtensile Bond Strength Evaluation

Table 4

Mean depth of study groups after different self-etching techniques.

Subgroups
(self-etching techniques)
HealthyMildModerateSevere

(1) Self-etch (SE)−2.11 ± 0.71−1.56 ± 0.61−1.62 ± 0.47−1.68 ± 0.59
(2) NaOCl/SE−2.41 ± 0.83−2.04 ± 0.43−2.01 ± 0.70−2.04 ± 0.80
(3) NaOCl/SE + NaAg−2.06 ± 0.32−1.96 ± 0.67−2.03 ± 0.41−2.70 ± −1.91

Results show means ± SD expressed in nanometers. An asterisk () indicates a statistically significant difference () with control subgroup by using ANOVA test.

We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.