Deviation from Regular Shape in the Early Stages of Formation of Strain-Driven 3D InGaAs/GaAs Micro/Nanotubes
Figure 3
Rolling distance () as a function of the etching time (); has been measured from SEM images (see the inset) on different μtubes giving error bars almost comparable to the spot size.