Research Article
Research on the Thermal Aging Behaviors of LDPE/TiO2 Nanocomposites
Table 3
Crystallinity of Pure-LDPE and LDPE/TiO2-0.5 samples aged different days.
| Aging days | Pure-LDPE | LDPE/TiO2-0.5 | | | | |
| 0 D | 147.18 | 50.12 | 154.84 | 52.74 | 14 D | 136.73 | 51.56 | 152.14 | 54.82 | 35 D | 131.50 | 44.78 | 141.99 | 48.36 | 56 D | 129.89 | 44.23 | 137.87 | 46.96 | 77 D | 115.91 | 39.47 | 134.03 | 45.65 |
|
|