Research Article

Polypropylene Carbon Nanotubes Nanocomposites: Combined Influence of Block Copolymer Compatibilizer and Melt Annealing on Electrical Properties

Figure 5

TEM micrograph of (a) PP50 after 10 min annealing time stained with RuO4; (b) PP0 stained with OsO4; (c) PP50 after 10 min annealing time stained with OsO4. See main text for further explanations.
(a)
(b)
(c)