Variation in oxidized (bleached) and reduced (blue) transmittance (%) with applied strains. The device was stretched uniaxially (as shown in Figure 3(b)). The transparency of the device varied by 9.89% in the oxidized state and 12.84% in the reduced states for strain rate of to .

Strain rate ()Transmittance (%)
OxidizedReduced

0.061.8441.48
0.1058.4443.77
0.1555.7246.81