(a) SEM and TEM images of silica-coated RC3 granule incorporated with Fe3O4 nanoparticle after calcination at 500°C for 2 hr. (b) XRD spectra of 50 nm Fe3O4 nanoparticle before and after heat treatment in air. (c) mHSP separation by a magnet after iodine absorption from the iodine contaminated water.