Discharge curves determined for (a) α-Ni(OH)2, (b) α1-Ni(OH)2@rGO, and (c) α2-Ni(OH)2@rGO at increasing current densities (8, 16, 32, 50, 75, and 100 A·g−1), (d) respective plots of the specific capacity as a function of the current density, and (e) discharge curves determined for α-Ni(OH)2, α1-Ni(OH)2@rGO, and α2-Ni(OH)2@rGO at 100 A·g−1.
(a)
(b)
(c)
(d)
(e)