Research Article
Effects of Sintering Temperature on the Morphology and Photoluminescence of Eu3+ Doped Zinc Molybdenum Oxide Hydrate
Figure 5
PL spectra of the precursors after thermal annealing at 200°C (a), 400°C (b), 600°C (c), and 800°C (d). The luminescent materials in (a) are the Eu3+ doped Zn5Mo2O11·5H2O whilst those in (b–d) are Eu3+ doped ZnMoO4 compounds. Inset: a zoom in the region 585–630 nm to show the split emissions of transitions 5D0 → 7F1 and 5D0 → 7F2.
(a) |
(b) |
(c) |
(d) |