Research Article

Effects of Sintering Temperature on the Morphology and Photoluminescence of Eu3+ Doped Zinc Molybdenum Oxide Hydrate

Figure 6

CIE chromaticity diagram of the colored PL from the precursors after thermal annealing at 200°C (a), 400°C (b), 600°C (c), and 800°C (d). The luminescent materials in (a) are Eu3+ doped Zn5Mo2O11·5H2O whilst those in (b–d) are Eu3+ doped ZnMoO4 compounds.