Research Article
Enhancement of Capacitive Performance in Titania Nanotubes Modified by an Electrochemical Reduction Method
Table 1
Voltage and time taken in the electrochemical reduction method of R-TNTs.
| Label | Voltage (V), time (s) |
| R-TNTs 4V30s | 4 V, 30 s | R-TNTs 5V30s | 5 V, 30 s | R-TNTs 6V30s | 6 V, 30 s | R-TNTs 7V30s | 7 V, 30 s | R-TNTs 5V10s | 5 V, 10 s | R-TNTs 5V20s | 5 V, 20 s | R-TNTs 5V40s | 5 V, 40 s |
|
|