Morphology and Electrochemical Characterization of Electrodeposited Nanocrystalline Ni-Co Electrodes for Methanol Fuel Cells

Figure 3

SEM micrographs of nanocrystalline Ni-Co alloys electrodeposited at 80 mA/cm2: (a) 15 min, (b) 20 min, and (c) 30 min.