Figure 8: UCL decays from 2H11/2 of Er3+ by monitoring the Er3+ emission at 523 nm under 980 nm excitation in LiGdF4:Yb3+/Er3+ nanocrystals, which are synthesized at , , and , 3 h, 4 h, and 5 h.