Samples(°)

UW56 (±3)
W+ZnO-9.9 (±0.4)0.5 (±0.3)1.7 (±1.2)10 (±1)68 (±6)
W+SH-4.1 (±1.9)1.6 (±0.8)6.5 (±0.6)8 (±2)88 (±5)
W+ZnO+SH-11.6 (±1.6)0.9 (±0.2)1.8 (±1.3)12 (±1)95 (±4)