Research Article

Influence of Bath Temperature and Deposition Time on Topographical and Optical Properties of Nanoparticles ZnS Thin Films Synthesized by a Chemical Bath Deposition Method

Table 1

Measured average ZnS nanoparticle diameters, heights, and surface roughness at bath temperature for different deposition times: 20, 30, 40, and 50 min.

Deposition time (min)Diameter (nm)Height (nm)Surface roughness (nm)

2086137
301061511
401201913
501272514